Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.0800 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
Pyrotek M-18 Compressible/Insulating Boards
ApplicationsTrough, ladle and launder linings High temperature gaskets Mill board substitute AdvantagesWater moldable Excellent thermal shock resistance High compressibility Excellent resistance to ..
Thermal Conductivity 0.0800 W/m-K

@Temperature 315 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 599 °F
Pyrotek M-13 Compressible/Insulating Boards
ApplicationsHigh temperature gaskets Non-conductive insulation Lid gaskets AdvantagesDurable Resistant to chemical attack Excellent mechanical strength Low air permeability Information provided by P..
Thermal Conductivity 0.0800 W/m-K

@Temperature 204 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 399 °F
Pyrotek Pyrocast L-30 Moldable Refractory
Pyrocast L-30 is a refractory moldable designed for use in contact with molten aluminum. Pyrocast L-30 has excellent workability for use as an insulating lining or patching material and is recommen..
Thermal Conductivity 0.0800 W/m-K

@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 752 °F
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..
Thermal Conductivity 0.0800 W/m-K

@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 752 °F
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..
Thermal Conductivity 0.0800 W/m-K

@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 752 °F
Mid-Mountain Materials CERMEX® PR1000-P Premium Grade Thermal Insulation Paper
Material: Non-respirable E-glass fibers Construction: Felted paper, organic binderInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.0800 W/m-K

@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-182
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
Thermal Conductivity 0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
4 pcf
Thermal Ceramics Cerablanket Blanket
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave..
Thermal Conductivity 0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
4 pcf
Thermal Ceramics Cerachem Blanket
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe..
Thermal Conductivity 0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
4 pcf
Thermal Ceramics Cerachrome Blanket
Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg..
Thermal Conductivity 0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
4 pcf
Thermal Ceramics Kaowool S Blanket
Kaowool S Blanket is produced from high quality spun fibers. It is available in a wide variety of densities and sizes, and offers a highly cost effective alternative to Cerablanket with its 2300°F ..
Thermal Conductivity 0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
Thermal Ceramics TR-2000 Block Insulation
TR-2000 SL Block Insulation is an asbestos-free insulation, manufactured from calcium silicate and reinforced with cellulose fibers. This item is versatile products available in a wide range of size..
Thermal Conductivity 0.0800 W/m-K

@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 752 °F
Zircar Ceramics AXHTM Alumina-Silica Insulation
ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a..
Thermal Conductivity 0.0800 W/m-K

@Temperature 525 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 977 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics ZAL-15AA Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.
Thermal Conductivity 0.0800 W/m-K

@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 752 °F
Zircar Zirconia ZYC Zirconia Cylinders Insulation
Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing ..
Thermal Conductivity 0.0800 W/m-K

@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 752 °F
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..
Thermal Conductivity 0.0800 W/m-K

@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 752 °F
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..
Thermal Conductivity 0.0800 W/m-K

@Temperature 800 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Zircar Refractory Composites ASPA-2 Alumina-Silica Fiber Paper
ASPA-2 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c..
Thermal Conductivity 0.0800 W/m-K

@Temperature 500 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 932 °F
Zircar Refractory Composites ASPA-880 Alumina-Silica Fiber Paper
ASPA-880 is a high temperature, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. It is made from shorter and smaller diameter fibers with a higher ..
Thermal Conductivity 0.0800 W/m-K

@Temperature 500 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 932 °F
parallel to thickness
Zircar Refractory Composites RS-3000 ALUMINA FELT
ZRCI Alumina Felt Type RS-3000 is 97% high purity alumina fiber, ceramic felt with less than 1% shot. Type RS-3000 is a strong, flexible material with fibers held together with an organic binder. It..
Thermal Conductivity 0.0800 W/m-K

@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C182
BNZ Materials Zelieblok 1900S Structural Ceramic Insulation
Information provided by BNZ Materials Inc.
Thermal Conductivity 0.0800 W/m-K

@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 752 °F
Zircar Zirconia ZYC Zirconia Cylinders Insulation
Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing ..
Thermal Conductivity 0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
Thermal Ceramics Kaomat Blanket
Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets...
Thermal Conductivity 0.0800 W/m-K

@Temperature 371 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 700 °F
Thermal Ceramics Kaomat SL Blanket
Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets...
Thermal Conductivity 0.0800 W/m-K

@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 500 °F
4 pcf
Thermal Ceramics Kaowool Blanket
Kaowool blanket is produced from kaolin, a naturally occurring alumina-silica fire clay. Kaowool, the world’s most recognizable name in ceramic fiber blanket, is available in a wide variety of dens..
Thermal Conductivity 0.0800 W/m-K

@Temperature 525 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 977 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics ZAL-15 Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.
Thermal Conductivity 0.0800 W/m-K

@Temperature 800 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Zircar Refractory Composites ASPA-1 Alumina-Silica Fiber Paper
ASPA-1 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c..
Thermal Conductivity 0.0800 W/m-K

@Temperature 870 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 1600 °F
Pyrotek M-12 Compressible/Insulating Boards
ApplicationsHigh temperature gaskets Furnace covers Trough lining AdvantagesLow density Good insulating ability Information provided by Pyrotek.