Material Notes:
ApplicationsHigh temperature gaskets Furnace covers Trough lining AdvantagesLow density Good insulating ability Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.210 g/cc
0.00759 lb/in³
Loss On Ignition 7.0 %
7.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000280 GPa

@Treatment Temp. 815 °C
0.0406 ksi

@Treatment Temp. 1500 °F
Compressive Strength 0.0310 MPa
4.50 psi
to 5% deformation
Thermal Properties Metric English Comments
Thermal Conductivity 0.0400 W/m-K

@Temperature 240 °C
0.278 BTU-in/hr-ft²-°F

@Temperature 464 °F
0.0500 W/m-K

@Temperature 425 °C
0.347 BTU-in/hr-ft²-°F

@Temperature 797 °F
0.0800 W/m-K

@Temperature 870 °C
0.555 BTU-in/hr-ft²-°F

@Temperature 1600 °F
Maximum Service Temperature, Air 1260 °C
2300 °F
Continuous
Component Elements Properties Metric English Comments
Al2O3 37 %
37 %
SiO2 51 %
51 %
Users viewing this material also viewed the following: