Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories LPCT-18PI Lance Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories LPCT-18PI Lance Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
0.00981 GPa

@Temperature 1350 °C,
Time 10800 sec
1.42 ksi

@Temperature 2460 °F,
Time 3.00 hour
0.018639 GPa

@Temperature 1500 °C,
Time 10800 sec
2.7034 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 34.3 MPa

@Temperature 110 °C,
Time 86400 sec
4980 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
70.6 MPa

@Temperature 1350 °C,
Time 10800 sec
10200 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
83.4 MPa

@Temperature 1500 °C,
Time 10800 sec
12100 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1800 °C
3270 °F
limited
Shrinkage 0.00 %

@Temperature 110 °C,
Time 86400 sec
0.00 %

@Temperature 230 °F,
Time 24.0 hour
0.50 %

@Temperature 1350 °C,
Time 10800 sec
0.50 %

@Temperature 2460 °F,
Time 3.00 hour
1.62 %

@Temperature 1500 °C,
Time 10800 sec
1.62 %

@Temperature 2730 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 93 %
93 %
SiO2 3.0 %
3.0 %
Descriptive Properties Value Comments
Installation Method Casting, Vibrating
Material Required for Estimating(kg/?) 3,200
Water Required for Casting(%) 6.0
Copyright © lookpolymers.com All Rights Reserved