Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Conductive Carbon Filled
Manufacturer Guarniflon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high wear strength. Enhanced chemical resistanceApplications: Bearings for high speed and when fast dissipation of electric charges is needed. Elastic bands for unlubricated compressors. Valve seats.Information provided by Guarniflon®
Physical Properties Metric English Comments
Density 2.04 - 2.10 g/cc
0.0737 - 0.0759 lb/in³
extruded; ASTM D792
2.05 - 2.11 g/cc
0.0741 - 0.0762 lb/in³
molded; ASTM D792
Deformation 2.5 - 4.0 %

@Pressure 13.7 MPa,
Time 86400 sec
2.5 - 4.0 %

@Pressure 1990 psi,
Time 24.0 hour
after 24hr relaxation; ASTM D621
5.0 - 6.0 %

@Pressure 13.7 MPa,
Time 86400 sec
5.0 - 6.0 %

@Pressure 1990 psi,
Time 24.0 hour
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 62 - 67
62 - 67
molded; ASTM D2240
62 - 67
62 - 67
extruded; ASTM D2240
Tensile Strength >= 12.0 MPa
>= 1740 psi
extruded; ASTM D4894, ASTM D4745
14.0 - 18.0 MPa
2030 - 2610 psi
molded; ASTM D4894, ASTM D4745
Elongation at Break >= 50 %
>= 50 %
extruded; ASTM D4745
70 - 120 %
70 - 120 %
molded; ASTM D4894
Compressive Yield Strength 7.00 - 9.00 MPa

@Strain 1.00 %
1020 - 1310 psi

@Strain 1.00 %
ASTM D695
Coefficient of Friction, Dynamic 0.11
0.11
ASTM D1894
K (wear) Factor 16.0 - 20.0 x 10-8 mm³/N-M
7.94 - 9.93 x 10-10 in³-min/ft-lb-hr
at PV 100; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 100 - 120 µm/m-°C
55.6 - 66.7 µin/in-°F
ASTM D696
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F