Material Notes:
ShinEtsu X30783 U is a phenyl (PVMQ) silicone product. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°C (148 to +500°F.)Typical Applications: Low temperature gaskets.Low temperature packing.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 48
48
Tensile Strength at Break 12.94 MPa
1877 psi
Elongation at Break 594 %
594 %
Tear Strength 34.4 kN/m
196 pli
Die B
Compression Set 23 %

@Temperature 180 °C,
Time 252000 sec
23 %

@Temperature 356 °F,
Time 70.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -100 °C
-148 °F
Descriptive Properties Value Comments
Cure Agent DBPH
Cure Type Press Cure