Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AC 80-10 Dense Refractory Brick Description: This bauxite base brick shows, due to the addition of CR2O3, a very good slag resistance.Remarks: This data represents average values, obtained from samples that were cut from standard .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AC 85-10 D Dense Refractory Brick Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AC 90-5 D Dense Refractory Brick Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast ACZ 85-5 D Dense Refractory Brick Description: Special low porosity quality with excellent resistance against alkali- and metal slags, a good volume stability and a high strength and elasticity at very high temperatures. Application.. |
|||
Maximum Service Temperature, Air | >= 1700 °C | >= 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 85 K Dense Refractory Brick Description: Corundum based bricks with a mullite bond. Application: rotating incinerator furnacesRemarks: This data represents average values, obtained from samples that were cut from standard bric.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AK 90 Dense Refractory Brick Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtaine.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast LP 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. The extremely low porosity results in a very good slag resistance, a good abrasion resistance and high.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast VIBRON 170 M GS (R) Dense Vibrating Refractory Castable Description: Vibron 170 M GS (R) is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sl.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
ICE Hot Pressed SiC Data provided by the manufacturer, International Ceramic Engineering. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AK 65 A Dense Refractory Brick Description: This andalusite based brick with a very pure mullite bond has a low alkali and iron content. In addition, it has a high creep resistance and is therefore used in applications where load.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AK 70 KP Dense Refractory Brick Description: A high quality phosphate bonded andalusite/corundum brick with very good volume stability. Also good slag resistance and thermal shock resistance. Remarks: This data represents average .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 85 KM Dense Refractory Brick Description: This brick based on mullite and corundum, is characterized by a very low porosity, high slag resistance, low creep and very good thermal shock resistance.Remarks: This data represents a.. |
|||
Maximum Service Temperature, Air | >= 1700 °C | >= 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 85 KP Dense Refractory Brick Description: This corundum based phosphate bond brick is characterized by a very low porosity, high slag resistance and high strength. Application: rotating incinerator furnaces.Remarks: This data r.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Sharadaa Ceramics PHOSTCAST 80 XL Phosphate Bonded Castables Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Sharadaa Ceramics REFCAST 80 High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Sharadaa Ceramics ZAP 005 Smart Cast Application Special Properties: Non-wetting, Slag and Hot Abrasion ResistanceIndustry: SteelApplication: Trough LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Sharadaa Ceramics ZAP 012 Smart Cast Application Special Properties: Patching At Hot Conditions, Easy InstallationIndustry: All IndustryApplication: All type of Rotary Kilns, AL/CU Melting Furnaces, Rolling Mills, Forgoing Furnaces, IncineratorsIn.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Intermittent |
Zircar Ceramics AL-30 Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Zircar Ceramics ALBF Alumina Bulk Fiber Alumina Bulk Fiber Type ALBF consists of long aluminum oxide fibers suited for the vacuum forming of low density shapes. The high alpha alumina content and addition of a grain growth inhibitor give .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Zircar Ceramics ALBF-1 Alumina Bulk Fiber Type ALBF-1 Alumina Bulk Fiber is a specially cleaned alumina fiber with relatively short fiber lengths. It is suitable for use in vacuum forming of high density rigid boards & shapes, in the reinfo.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Zircar Ceramics SALI Alumina Insulation SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength.Information provi.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Intermittent |
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Intermittent |
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Intermittent |
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | NO-LOAD COND. |
CoorsTek ADD-96 96% Alumina |
|||
Maximum Service Temperature, Air | >= 1700 °C | >= 3090 °F | |
China-Yixing Longly Refractories Zirconia Ceramics LONGLY provides a multitude of zirconia products including balls, plates, tubes, rods and etc. by adopting magnesia, calcia or yttria stabilized zirconia powder as raw material through dry pressing,.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Intermittent |
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |