Gouda Vuurvast AK 85 KP Dense Refractory Brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast AK 85 KP Dense Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This corundum based phosphate bond brick is characterized by a very low porosity, high slag resistance and high strength. Application: rotating incinerator furnaces.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.29 g/cc
0.0827 lb/in³
Apparent
Porosity <= 15 %
<= 15 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 80.0 MPa
11600 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 2.10 W/m-K

@Temperature 1100 °C
14.6 BTU-in/hr-ft²-°F

@Temperature 2010 °F
2.30 W/m-K

@Temperature 650 °C
16.0 BTU-in/hr-ft²-°F

@Temperature 1200 °F
2.60 W/m-K

@Temperature 100 °C
18.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air >= 1700 °C
>= 3090 °F
Deformation under load - t<sub>a</sub>
1750 °C
3180 °F
Component Elements Properties Metric English Comments
Al2O3 85 %
85 %
Fe2O3 <= 0.50 %
<= 0.50 %
SiO2 13 %
13 %
Descriptive Properties Value Comments
Segercone 39
Thermal Shock Resistance 30 cycles
DIN 51068