Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast AK 90 Dense Refractory Brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast AK 90 Dense Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 3.05 g/cc
0.110 lb/in³
Apparent
Porosity 18 %
18 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 85.0 MPa
12300 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 2.20 W/m-K

@Temperature 1100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 2010 °F
2.30 W/m-K

@Temperature 650 °C
16.0 BTU-in/hr-ft²-°F

@Temperature 1200 °F
2.60 W/m-K

@Temperature 100 °C
18.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1700 °C
3090 °F
1750 °C
3180 °F
Deformation under load - t<sub>a</sub>
Component Elements Properties Metric English Comments
Al2O3 90 %
90 %
Fe2O3 <= 0.50 %
<= 0.50 %
SiO2 9.5 %
9.5 %
Descriptive Properties Value Comments
Segercone 40
Thermal Shock Resistance 30 cycles
DIN 51068
Copyright © lookpolymers.com All Rights Reserved