Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 899 °C | 1650 °F | Upper limit of working range |
Heatbath/Park Nu-Sal High Speed Hardening Salt This barium-free salt is the most economical and most commonly used neutral salt for heat treating performed within its working range. It is non-hygroscopic and relatively non-corrosive to metal an.. |
|||
Maximum Service Temperature, Air | 899 °C | 1650 °F | Upper limit of working range |
Heatbath/Park Nu-Sal Neutral Salt This barium-free salt is the most economical and most commonly used neutral salt for heat treating performed within its working range. It is non-hygroscopic and relatively non-corrosive to metal an.. |
|||
Maximum Service Temperature, Air | 899 °C | 1650 °F | Upper limit of working range |
Heatbath/Park Nu-Sal Steel Brazing Neutral Salt The most economical salt for brazing performed within its working range. Silver and brass brazing are commonly done in Nu-Sal. It is non-hygroscopic and relatively non-corrosive to metal and fixture.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group ISOPERLOR 550P Perlite Insulating Brick & Block ISOPERLOR perlite insulating bricks & blocks have the following characteristics: Max. service temperature 900°C (1652°F)Back-up insulation onlyExcellent insulating propertiesVery lightweight a.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group Moler 10 Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group Moler 5 Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group Moler BB-BLOCK Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group Moler BB-Filler Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group Moler BF-BLOCK Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group Moler HIPOR Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group Moler HIPOROS Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group Moler POROS Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group Moler SUPRA Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group SKAMOCAST 112-80 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Skamol Group Skamol M-20 Insulating Mortar SKAMOL insulating mortars have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grad.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | Continuous Use |
Goodfellow Alumino-silicate Glass Ceramic SiO2 57/Al2O3 36/CaO/MgO/BaOPorous ceramics can be used as filters and for the controlled release of volatile chemicals. In this material, Alumino-Silicate particles are found in a glassy matrix. Th.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | Continuous Use, with 304 Stainless Wire Reinforcement |
Zircar Ceramics AS-1260 Alumina-Silica Textile Multiple forms of ceramic fiber textiles made of reinforced yarn. Amazingly strong, they are useful as gasketing, insulation and fire protection to temperatures of 1260°C (2300°F).Information pro.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Zircar Refractory Composites RS-B ALUMINA-SILICA MOLDABLE ZIRCAR Alumina-Silica Insulating Blanket Type RS-B Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped .. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | Continuous |
Corning Vycor® 7950 Red Glass Used to reduce the light of quartz lamps (blocks most visible white light while transmitting IR). One specific use is blocking glare from heating units.Special Features:Superior optical qualityTigh.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Eifeler Coatings Technology EXXTRAL® blue PVD Coating Key Characteristics: extreme wear resistance at high temperature, excellent oxidation resistancePrimary Applications: cutting extremely abrasive or hard materials; machining of hardened steel >55HRc.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Eifeler Coatings Technology SISTRAL® AlTiN PVD Coating Key Characteristics: extreme wear resistance at high temperature, excellent oxidation resistancePrimary Applications: excellent choice for cutting under extreme conditions (hard abrasive materials, .. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Eifeler Coatings Technology TIGRAL AlCrTiN PVD Coating Key Characteristics: high warm hardness, very high oxidation resistance, high protection against abrasive wearPrimary Applications: warm forming, hot forging, and die casting; coating for milling wi.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | Continuous |
Corning Vycor® 7907 UV-Blocking Glass Vycor-UV™ is cerium-doped and provides homogeneous absorption of UV-B and UV-C.Special Features:Superior optical qualityTight dimensional controlThermal and chemical properties ideally suited to hi.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | Operating Temperature |
California Fine Wire Stablohm 675 Nickel, Chromium and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Maximum Service Temperature, Air | 899 °C | 1650 °F | oxidation resistance is excellent and low scaling rate at this temp |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317L (UNS S31703) Allegheny Ludlum's 317L™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless s.. |
|||
Maximum Service Temperature, Air | 899 °C | 1650 °F | oxidation resistance is excellent and low scaling rate at this temp |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LX™ (UNS S31725) Allegheny Ludlum's 317LX™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless .. |
|||
Maximum Service Temperature, Air | 899 °C | 1650 °F | Excellent oxidation and scaling resistance to this temp. |
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Maximum Service Temperature, Air | 899 °C | 1650 °F | Excellent oxidation and scaling resistance to this temp. |
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
CeramTec 848 Zirconia, ZrO2•MgO Tetragonal zirconia exhibits high flexural strength and superior low temperature stability. It features higher impact strength and erosive wear resistance as compared to alumina. 848 TTZP (yellow) i.. |
|||
Maximum Service Temperature, Air | 900 °C | 1650 °F | |
Chesterton 783 ACR Anti-Seize Compound Description: Chesterton® 783 ACR represents the newest generation of anti-seize compound. A proprietary blend of ultra-fine inorganic solid lubricants, 783 ACR can be used under extremely severe co.. |