Skamol Group Skamol M-20 Insulating Mortar

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Skamol Group
Trade Name Skamol
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Skamol Group Skamol M-20 Insulating Mortar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SKAMOL insulating mortars have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grades in various applicationsGood insulation valuesOutstanding bonding properties within max. service temperature rangeWater-retentive properties for quick and easy laying of dry bricks/blocks/slabs.Combined air and heat-setting.Information provided by Skamol.
Physical Properties Metric English Comments
Bulk Density 0.529 g/cc
0.0191 lb/in³
As Supplied
0.897 g/cc
0.0324 lb/in³
Dried at 110°C (230°F)
Loss On Ignition 6.00 %

@Temperature 1025 °C
6.00 %

@Temperature 1877 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 900 °C
1650 °F
Component Elements Properties Metric English Comments
Al2O3 11 %
11 %
CaO 1.0 %
1.0 %
Fe2O3 5.5 %
5.5 %
K2O 1.3 %
1.3 %
MgO 1.0 %
1.0 %
Na2O 5.0 %
5.0 %
SiO2 67 %
67 %
TiO2 1.0 %
1.0 %
Processing Properties Metric English Comments
Moisture Content 2.0 %
2.0 %
as supplied
Descriptive Properties Value Comments
Binder Silicate
Mixing Water Usage 22.5 liters to 25kg
Package Weight 25 kg
Unit weight, all included. Plastic sack with dry mix.
Pyrometric Cone Equivalent 1040°C
ASTM C24-89, ORTON cones
Recommended Joint Thickness 3.0-5.0 mm
Setting Mechanism air and heat-setting
Type dry mix
Usage 3 kg
Quantity to fix 1m<sup>2</sup> (11 ft<sup>2</sup>) of Slabs
65 kg
Quantity to set 1m<sup>3</sup> (35.31 ft<sup>3</sup>) of Bricks