Maximum Service Temperature, Air 899 °C
1650 °F
Upper limit of working range
Heatbath/Park Nu-Sal High Speed Hardening Salt
This barium-free salt is the most economical and most commonly used neutral salt for heat treating performed within its working range. It is non-hygroscopic and relatively non-corrosive to metal an..
Maximum Service Temperature, Air 899 °C
1650 °F
Upper limit of working range
Heatbath/Park Nu-Sal Neutral Salt
This barium-free salt is the most economical and most commonly used neutral salt for heat treating performed within its working range. It is non-hygroscopic and relatively non-corrosive to metal an..
Maximum Service Temperature, Air 899 °C
1650 °F
Upper limit of working range
Heatbath/Park Nu-Sal Steel Brazing Neutral Salt
The most economical salt for brazing performed within its working range. Silver and brass brazing are commonly done in Nu-Sal. It is non-hygroscopic and relatively non-corrosive to metal and fixture..
Maximum Service Temperature, Air 899 °C
1650 °F
oxidation resistance is excellent and low scaling rate at this temp
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317L (UNS S31703)
Allegheny Ludlum's 317L™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless s..
Maximum Service Temperature, Air 899 °C
1650 °F
oxidation resistance is excellent and low scaling rate at this temp
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LXN™ (UNS S31726)
Allegheny Ludlum's 317LXN™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless..
Maximum Service Temperature, Air 899 °C
1650 °F
oxidation resistance is excellent and low scaling rate at this temp
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LX™ (UNS S31725)
Allegheny Ludlum's 317LX™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless ..
Maximum Service Temperature, Air 899 °C
1650 °F
Excellent oxidation and scaling resistance to this temp.
ATI Allegheny Ludlum Type 317 Stainless Steel, UNS S31700
This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels ..
Maximum Service Temperature, Air 899 °C
1650 °F
Excellent oxidation and scaling resistance to this temp.
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600
This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels ..
Maximum Service Temperature, Air 899 °C
1650 °F
Excellent oxidation and scaling resistance to this temp.
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603
This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels ..