Material Notes:
Multiple forms of ceramic fiber textiles made of reinforced yarn. Amazingly strong, they are useful as gasketing, insulation and fire protection to temperatures of 1260°C (2300°F).Information provided by Zircar Ceramics.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 600 °C
1110 °F
Continuous Use, with Glass Fiber Reinforcement
900 °C
1650 °F
Continuous Use, with 304 Stainless Wire Reinforcement
1260 °C
2300 °F
Component Elements Properties Metric English Comments
Al2O3 47 %
47 %
SiO2 53 %
53 %
Descriptive Properties Value Comments
Ceramic Fiber 82 %
not including reinforcement
Color Off White
Organic Fiber 18 %
not including reinforcement