Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals BioBrass® UNS C27000 Copper-Zinc Alloy Finished product available as wire, rod, or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extrude.. |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals BioBrass® UNS C27450 Copper-Zinc Alloy Finished product available as wire or tube.Chicago Extruded Metal temper code: H04Information provided by Chicago Extruded Metals |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals BioBrass® UNS C46400 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, wire, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Met.. |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals UNS C33500 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in bars.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals UNS C34000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals UNS C34500 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in rods.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals UNS C35000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02, H04Information provided by Chicago Extruded Metals |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals UNS C35300 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02, H04Information provided by Chicago Extruded Metals |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals UNS C36000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals UNS C48200 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Metals |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals UNS C48500 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals UNS C36010 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, wire, rod or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Thermal Conductivity | 116 W/m-K | 805 BTU-in/hr-ft²-°F | |
California Fine Wire Nickel Alloy 30 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Thermal Conductivity | 116 W/m-K | 804 BTU-in/hr-ft²-°F | |
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual .. |