Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

California Fine Wire Nickel Alloy 30 Copper Nickel Resistance Wire

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Copper Alloy
Manufacturer California Fine Wire
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Nickel Alloy 30 Copper Nickel Resistance Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.89 g/cc
0.321 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 207 MPa
30000 psi
Annealed
414 MPa
60000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 16.4 µm/m-°C

@Temperature 20.0 °C
9.11 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.385 J/g-°C

@Temperature 20.0 °C
0.0920 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 116 W/m-K
805 BTU-in/hr-ft²-°F
Melting Point 1100 °C
2012 °F
Maximum Service Temperature, Air 600 °C
1110 °F
Operating Temperature
Component Elements Properties Metric English Comments
Copper, Cu 98 %
98 %
Nickel, Ni 2.0 %
2.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000499 ohm-cm
0.00000499 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic None
Temperature Coefficient of Resistance 0.0013 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.014
Copyright © lookpolymers.com All Rights Reserved