Material Notes:
Finished product available as wire or tube.Chicago Extruded Metal temper code: H04Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.58 g/cc
0.310 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 68
68
Tensile Strength 434 MPa
63000 psi
Tensile Strength, Yield 324 MPa
47000 psi
Elongation at Break 25 %
25 %
Machinability 70 %
70 %
UNS C36000 (free-cutting brass) = 100%
Thermal Properties Metric English Comments
Thermal Conductivity 116 W/m-K
804 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 60 - 65 %
60 - 65 %
Iron, Fe 0.35 %
0.35 %
Lead, Pb 0.25 %
0.25 %
Other, total 0.50 %
0.50 %
Zinc, Zn 33.9 - 38.9 %
33.9 - 38.9 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000639 ohm-cm
0.00000639 ohm-cm