Chicago Extruded Metals BioBrass® UNS C27000 Copper-Zinc Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Chicago Extruded Metals (CXM)
Trade Name BioBrass®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chicago Extruded Metals BioBrass® UNS C27000 Copper-Zinc Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Finished product available as wire, rod, or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.47 g/cc
0.306 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 55
55
Tensile Strength 331 - 827 MPa
48000 - 120000 psi
Tensile Strength, Yield 110 - 276 MPa
16000 - 40000 psi
Elongation at Break 3.0 - 66 %
3.0 - 66 %
Machinability 30 %
30 %
UNS C36000 (free-cutting brass) = 100%
Thermal Properties Metric English Comments
Thermal Conductivity 116 W/m-K
804 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 63 - 68.5 %
63 - 68.5 %
Iron, Fe 0.070 %
0.070 %
Lead, Pb 0.090 %
0.090 %
Other, total 0.30 %
0.30 %
Zinc, Zn 31.04 - 36.54 %
31.04 - 36.54 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000639 ohm-cm
0.00000639 ohm-cm