Material Notes:
Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, wire, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.41 g/cc
0.304 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 55 - 95
55 - 95
Tensile Strength 386 - 607 MPa
56000 - 88000 psi
Tensile Strength, Yield 172 - 455 MPa
25000 - 66000 psi
Elongation at Break 18 - 47 %
18 - 47 %
Machinability 30 %
30 %
UNS C36000 (free-cutting brass) = 100%
Thermal Properties Metric English Comments
Thermal Conductivity 116 W/m-K
804 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 59 - 62 %
59 - 62 %
Iron, Fe 0.10 %
0.10 %
Lead, Pb 0.20 %
0.20 %
Other, total 0.40 %
0.40 %
Tin, Sn 0.50 - 1.0 %
0.50 - 1.0 %
Zinc, Zn 36.3 - 39.8 %
36.3 - 39.8 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000663 ohm-cm
0.00000663 ohm-cm