Thermal Properties Metric English Comments
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
ASTM C158
Rogers Corporation Bisco™ HT-820 Cellular Silicone Foam
Firm grade silicone sponge. UL recognized for flame retardance.Applications: Gaskets where higher closure force is available or necessary, Cushions in heavier-load applicationsGasketing and sealing..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
DIN.52612
Omnia Plastica PVDF Kynar
PVDF is a relatively new fluoropolymer. Like the other fluoropolymers, its best feature is its chemical resistance. The mechanical features of PVDF are notably higher than PTFE and it does not suffe..
Thermal Conductivity 0.110 - 0.150 W/m-K

@Temperature 50.0 - 400 °C
0.763 - 1.04 BTU-in/hr-ft²-°F

@Temperature 122 - 752 °F
Pyrotek Firefly 800 Roller & Furnace Cladding Material
Firefly 800 is a beige asbestos-free material made from high-quality shot-free mineral wool and inert fillers. Rollers made of Firefly 800 are constructed to resist breakage in handling service. F..
Thermal Conductivity 0.110 - 0.150 W/m-K
0.763 - 1.04 BTU-in/hr-ft²-°F
Pyrotek U-1 Compressible Board
U-1 is a high-temperature millboard that is easily cut, punched and shaped. It works well as a roll-cladding material and as compressible gasketing. A unique characteristic of the asbestos-free bo..
Thermal Conductivity 0.110 - 0.300 W/m-K
0.763 - 2.08 BTU-in/hr-ft²-°F
Average value: 0.182 W/m-K Grade Count:62
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Trelleborg Fillite® 160 Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Trelleborg Fillite® 160W Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Trelleborg Fillite® 52/7S (355) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Trelleborg Fillite® FG (300) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Trelleborg Fillite® 106 Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Trelleborg Fillite® 300W Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic
HYTAC-FLX has been improved for optimum performance in transparent applications. The enhanced formulation is easy to polish and results in minimal to no scratches with transparent sheet materials. ..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Dow Corning XIAMETER® PMCPPMX-0210 Silicone Fluid 100CS
Is chemically equivalent to DOW CORNING® 210H FLUID 100CS. This product is a heat stabilized polydimethlysiloxane, used for heat transfer.Information provided by Dow Corning
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Trelleborg Fillite® PG (300LF) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Thermal Conductivity 0.110 W/m-K
0.763 BTU-in/hr-ft²-°F
Hippe PVDF