Thermal Properties Metric English Comments
Thermal Conductivity 0.110 - 0.150 W/m-K

@Temperature 50.0 - 400 °C
0.763 - 1.04 BTU-in/hr-ft²-°F

@Temperature 122 - 752 °F
Pyrotek Firefly 800 Roller & Furnace Cladding Material
Firefly 800 is a beige asbestos-free material made from high-quality shot-free mineral wool and inert fillers. Rollers made of Firefly 800 are constructed to resist breakage in handling service. F..
Thermal Conductivity 0.110 - 0.150 W/m-K
0.763 - 1.04 BTU-in/hr-ft²-°F
Pyrotek U-1 Compressible Board
U-1 is a high-temperature millboard that is easily cut, punched and shaped. It works well as a roll-cladding material and as compressible gasketing. A unique characteristic of the asbestos-free bo..
Thermal Conductivity 0.150 - 0.150 W/m-K

@Temperature 40.0 - 40.0 °C
1.04 - 1.04 BTU-in/hr-ft²-°F

@Temperature 104 - 104 °F
Average value: 0.150 W/m-K Grade Count:13
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..