Pyrotek Firefly 800 Roller & Furnace Cladding Material

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name Firefly
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Firefly 800 Roller & Furnace Cladding Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Firefly 800 is a beige asbestos-free material made from high-quality shot-free mineral wool and inert fillers. Rollers made of Firefly 800 are constructed to resist breakage in handling service. Firefly 800 exhibits excellent flame and heat resistance with virtually no dimensional changes. It has self-cleaning properties and has no shot or abrasive elements to scratch hot glass.ApplicationsFurnace lining Roller cladding material Gaskets and seals AdvantagesAsbestos-free Excellent thermal stability High mechanical strength Non-abrasive Wet moldable Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.875 g/cc
0.0316 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1.80 MPa

@Temperature 500 °C
261 psi

@Temperature 932 °F
3.50 MPa

@Temperature 800 °C
508 psi

@Temperature 1470 °F
4.00 MPa

@Temperature 23.0 °C
580 psi

@Temperature 73.4 °F
Compressive Strength 21.0 MPa
3050 psi
35-45%
Thermal Properties Metric English Comments
Thermal Conductivity 0.110 - 0.150 W/m-K

@Temperature 50.0 - 400 °C
0.763 - 1.04 BTU-in/hr-ft²-°F

@Temperature 122 - 752 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
Shrinkage 0.250 %

@Temperature 1000 °C
0.250 %

@Temperature 1830 °F
Width
0.890 %

@Temperature 1000 °C
0.890 %

@Temperature 1830 °F
Length
1.90 %

@Temperature 1000 °C
1.90 %

@Temperature 1830 °F
Thickness