Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C

@Thickness 3.18 mm
151 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Packaging 161J1-3V Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C

@Thickness 6.35 mm
151 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Packaging M2288 Polyvinyl Chloride, Rigid (PVC, Rigid)
Opaque sheet extrusion compound.Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
Unannealed; ASTM D648
Multibase Nylex™ 2185 CR Polyamide + PP
Forms: PelletsFeatures:Chemical Resistance, GoodInformation provided by Multibase
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C

@Thickness 3.18 mm
151 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Packaging PK9 WHITE 1082 Polyvinyl Chloride, Rigid (PVC, Rigid)
The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 66.1 - 196 °C
151 - 385 °F
Average value: 87.9 °C Grade Count:119
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
Unannealed; ISO 75A-1, -2
LyondellBasell Hostacomâ„¢ TKS709D Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ TKS709D medium high melt flow, 1,600 MPa flexural modulus, UV-stabilized, thermoplastic elastomeric olefin (TEO) resin has an excellent combination of properties and proc..
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
Unannealed; ASTM D648
Techmer ES Plastiblend® PA6/10 BK Nylon 610
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
unannealed (0.125 in); ASTM D648
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures ..
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
Aclo Accuguard ABS ABS860V0L Flame Retardant
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
Aclo Accutech Polypropylene Copolymer CP0436W40L Wollastonite Reinforced
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
Aclo Accutech Polypropylene Homopolymer HP0336W20L1 Wollastonite Reinforced
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
ASTM D-648
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
ASTM D-648
Axiall 7803 Rigid PVC, Extrusion High Impact Profile
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
unannealed; ASTM D-648
Axiall 8607 Rigid PVC, Extrusion
Georgia Gulf 8607 is a special purpose pelletized compound formulated for high impact, rigid extrusion profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.