Material Notes:
Georgia Gulf 8607 is a special purpose pelletized compound formulated for high impact, rigid extrusion profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 78.5
78.5
ASTM D-2240
Tensile Strength, Yield 39.2 MPa
5680 psi
ASTM D-638
Tensile Modulus 2.54 GPa
368 ksi
ASTM D-638
Flexural Strength 63.4 MPa
9200 psi
ASTM D-790
Flexural Modulus 1.92 GPa
279 ksi
ASTM D-790
Izod Impact, Notched 2.88 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
5.40 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
11.6 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
21.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 156 kJ/m²
74.3 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C
162 °F
unannealed; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
unannealed; ASTM D-648
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F
Descriptive Properties Value Comments
Cell Classification 16343