Material Notes:
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
MD; ASTM D955
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92
92
ASTM D785
Tensile Strength at Break 27.0 MPa
3920 psi
ASTM D638
Tensile Strength, Yield 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Flexural Strength 57.0 MPa
8270 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 3.58 J/cm
6.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.2 °C
171 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F
Flammability, UL94 5VA
5VA
1/16 UL File #E56070, Rating of 5VA with 1/10 FSA File #LS66844
5VA
5VA
Rating of 5VA with 1/10 FSA File #LS66844