Aclo Accutech Polypropylene Copolymer CP0436W40L Wollastonite Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0436W40L Wollastonite Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
MD; ASTM D955
Melt Flow 11 g/10 min
11 g/10 min
ASTM D1238
Ash 40 %
40 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 50
50
ASTM D785
Tensile Strength at Break 17.0 MPa
2470 psi
ASTM D638
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 18 %
18 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 2.699 GPa
391.5 ksi
ASTM D638
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
Flexural Modulus 2.699 GPa
391.5 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
151 °F