Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifaxâ„¢ CB276 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB276 very high melt flow, 1,200 MPa flexural modulus, UV-stabilized, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F | Unannealed; ISO 75-2/Af |
Styron INSPIREâ„¢ T710-25 ES PolyPropylene Resin DA Thermoplastic Polyolefin Dow T710-25 ES Polypropylene Resin DAâ„¢ is a high impact TPO with enhanced flow, scratch and mar, and surface aesthetics for excellent molded-in-color appearance for automotive interior applicat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® TPU/E 0140 Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F | ISO 75-2/A |
ExxonMobil Exxtral™ BMU 131 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, good surface appearance and good weatherability designed for automotive exterior .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CNK 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection or extrusion automotive applications with low melt and excellent low temperature impact. Availability: Africa &.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CNR 012 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive applications. Availability: Africa & Middle East, Asia Pacific, Europe South America and Nort.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CNU 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good UV resistance designed for automotive exterior applications. Availability: Africa & Middle East, Asia Pacific, Europe, South.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F | |
Aclo Accucomp Polypropylene CPO402V Automotive Approved Copolymer Extrusion Grade |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F | |
Aclo Accucomp Polypropylene CPO406L Copolymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F | |
Aclo Accuguard Polypropylene CP1467V2CSL Copolymer Flame Retardant Copper Stabilized |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 °C | 118 °F | |
BCC Products BC 4558 Polyester Filler Paste BC4558 is a unique quickset paste designed for aircraft use in making fast repairs to damaged metal surfaces. Also recommended for use in edge filling honeycomb core and foam core composite panels. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 - 110 °C | 118 - 230 °F | Average value: 60.4 °C Grade Count:34 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |