Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styron INSPIREâ„¢ T710-25 ES PolyPropylene Resin DA Thermoplastic Polyolefin

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Styron
Trade Name INSPIRE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron INSPIREâ„¢ T710-25 ES PolyPropylene Resin DA Thermoplastic Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow T710-25 ES Polypropylene Resin DAâ„¢ is a high impact TPO with enhanced flow, scratch and mar, and surface aesthetics for excellent molded-in-color appearance for automotive interior applications. Main Characteristics: It has a tiger stripe freeSlip agentApproved on DaimlerChrysler MS-DB500Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010
Physical Properties Metric English Comments
Density 0.897 g/cc
0.0324 lb/in³
ASTM D792
Melt Flow 27 g/10 min

@Load 2.16 kg,
Temperature 230 °C
27 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.6 MPa
2840 psi
ISO 527-2/50
Flexural Modulus 0.9660 GPa
140.1 ksi
2 mm/min; ISO 178
Charpy Impact, Notched 0.540 J/cm²

@Temperature -40.0 °C
2.57 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eA
4.90 J/cm²

@Temperature 23.0 °C
23.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Dart Drop, Total Energy 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
6.60 m/sec, Ductile; ASTM D3763
46.0 J

@Temperature -29.0 °C
33.9 ft-lb

@Temperature -20.2 °F
6.60 m/sec, Ductile; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.2 °C
171 °F
Unannealed; ISO 75-2/Bf
Deflection Temperature at 1.8 MPa (264 psi) 47.8 °C
118 °F
Unannealed; ISO 75-2/Af
Users viewing this material also viewed the following: