ExxonMobil Exxtral™ CNR 012 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ CNR 012 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive applications. Availability: Africa & Middle East, Asia Pacific, Europe South America and North America Features: DuctileGood Creep ResistanceGood Surface FinishHigh Impact ResistanceLow to No FoggingUses: Automotive Applications Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
ISO 527-2
Elongation at Break >= 400 %
>= 400 %
ISO 527-2
Elongation at Yield 10 %
10 %
ISO 527-2
Tensile Modulus 1.00 GPa
145 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.441 J/cm²

@Temperature -20.0 °C
2.10 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.651 J/cm²

@Temperature 0.000 °C
3.10 ft-lb/in²

@Temperature 32.0 °F
ISO 179
1.60 J/cm²

@Temperature 22.8 °C
7.60 ft-lb/in²

@Temperature 73.0 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.2 °C
171 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 47.8 °C
118 °F
ISO 75-2/A