Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ BMU 131 Performance Polyolefin

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ BMU 131 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, good surface appearance and good weatherability designed for automotive exterior applications.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/ToughnessDuctileGood Surface FinishGood UV ResistanceGood Weather ResistanceLow Temperature Impact Resistance Uses: Automotive BumperAutomotive Exterior PartsAutomotive Exterior TrimProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.0 MPa
1890 psi
ISO 527-2
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527-2
Elongation at Break 54 %
54 %
ISO 527-2
Elongation at Yield 4.0 %
4.0 %
ISO 527-2
Tensile Modulus 1.24 GPa
180 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.609 J/cm²

@Temperature -30.0 °C
2.90 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
0.798 J/cm²

@Temperature -20.0 °C
3.80 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 47.8 °C
118 °F
ISO 75-2/A
Users viewing this material also viewed the following: