Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -45.0 - -40.0 °C | -49.0 - -40.0 °F | Average value: -43.3 °C Grade Count:3 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m.. |
|||
Brittleness Temperature | -100 - -40.0 °C | -148 - -40.0 °F | Average value: -84.7 °C Grade Count:42 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Brittleness Temperature | -70.0 - -40.0 °C | -94.0 - -40.0 °F | Average value: -61.3 °C Grade Count:30 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |