Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.900 - 1.09 g/cc
0.0325 - 0.0394 lb/in³
Average value: 0.980 g/cc Grade Count:10
Melt Flow 0.500 - 2.30 g/10 min
0.500 - 2.30 g/10 min
Average value: 0.865 g/10 min Grade Count:10
Mechanical Properties Metric English Comments
Hardness, Shore D 40.0 - 65.0
40.0 - 65.0
Average value: 55.4 Grade Count:10
Tensile Strength, Ultimate 17.0 - 32.4 MPa
2470 - 4700 psi
Average value: 25.1 MPa Grade Count:10
Tensile Strength, Yield 11.9 - 20.5 MPa
1730 - 2970 psi
Average value: 18.0 MPa Grade Count:4
Elongation at Break 500 - 700 %
500 - 700 %
Average value: 610 % Grade Count:5
Flexural Modulus 0.138 - 1.77 GPa
20.0 - 257 ksi
Average value: 0.736 GPa Grade Count:10
Izod Impact, Notched 0.320 - 4.38 J/cm
0.599 - 8.21 ft-lb/in
Average value: 1.67 J/cm Grade Count:4
Gardner Impact 34.0 - 36.0 J

@Temperature -30.0 - -30.0 °C
25.1 - 26.6 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 36.2 J Grade Count:6
Tear Strength 80.0 - 120 kN/m
456 - 685 pli
Average value: 98.2 kN/m Grade Count:5
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 57.0 - 92.0 °C
135 - 198 °F
Average value: 79.5 °C Grade Count:4
Brittleness Temperature -45.0 - -40.0 °C
-49.0 - -40.0 °F
Average value: -43.3 °C Grade Count:3