Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
RheTech Products RCC220-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: I/P hush panelsSplash shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
LyondellBasell Hostacomâ„¢ BG722AC Polypropylene Copolymer Description: Hostacomâ„¢ BG722AC medium high melt flow, 1,700 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer is designed with an excellent balance of stiffness, impact r.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ISO 75B-1, -2 |
LyondellBasell Hostacomâ„¢ BR712GC Polypropylene Copolymer Description: Hostacomâ„¢ BR712GC conventional melt flow, 1,300 MPa flexural modulus, UV-stabilized, mineral-filled polypropylene copolymer has an excellent balance of stiffness, impact and weathe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS FR AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ASA 814 GY Availability: North AmericaForms: PelletsFeatures: Good Weather ResistanceAppearance: GrayInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 7000 Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8007 Availability: North AmericaForms: PelletsFeatures: General Purpose and High FlowInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® ABS AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® ABS FR AS BN Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | Unannealed, 0.125 in; ASTM D648 |
Chase Plastics CP Pryme® A100HF ABS Features: High FlowGeneral PurposeGood toughnessForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C @Thickness 3.17 mm |
192 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
Chase Plastics CP Pryme® A100HI ABS Molding Resin, High Impact Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ISO 75-2/Bf |
ExxonMobil Exxtral™ BMV 102W Performance Polyolefin Product Description: Polyolefin injection molding compound with high flow, good low-temperature impact resistance, and excellent processability for painted, partial painted, and molded-in-color auto.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
Clariant Renol SB83642580 ASA Polymer Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437M20L Mica Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | annealed; ASTM D648 |
Arkema Group Solarkote® PB Acrylic For PVC/acrylic alloys Information provided by Arkema Group |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
Americas Styrenics EA3400 High Heat Crystal Polystyrene Product CharacteristicsLess than 300 parts per million residual volatiles with minimal taste and odor transferExcellent clarity and colorGood toughnessFood Contact CompliantTypical ApplicationsCap l.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
Americas Styrenics EA6740 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
Americas Styrenics STYRON A-TECH® 1115 High Impact Polystyrene Product CharacteristicsHigh Gloss/High ImpactConsistent colorabilityEasy processingFood Contact CompliantTypical ApplicationsCustom high Gloss Extruded SheetRefrigeration accessoriesSmall Appliances.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene Product CharacteristicsMedium heat resistanceMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsMedicalPackaging/disposablesInformation provided by AmericasStyrenics LLC. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | unannealed; injection molded; ASTM D648 |
Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin STYRON™ 668 is a general purpose polystyrene with medium flow and a balance of heat resistance and stiffness characteristics that make it suitable for applications such as CD jewel boxes. STYRON™.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | annealed; ASTM D648 |
Arkema Group Solarkote® A200 Acrylic Superior UV protection and weatherability, ASTM Classification PMMA 0233V1Information provided by Arkema Group |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
Americas Styrenics STYRON® 487R High Impact Polystyrene Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by Amer.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | unannealed; injection molded; ASTM D648 |
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C | 192 °F | ASTM D648 |
Ineos H19G-00 Polypropylene Homopolymer This is a homopolymer designed for extrusion processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsContinuous Filament YarnBCFSta.. |