Aclo Accutech Polypropylene Copolymer CP0437M20L Mica Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Mica Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0437M20L Mica Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
MD; ASTM D955
Melt Flow 18 g/10 min
18 g/10 min
ASTM D1238
Ash 20 %
20 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 42
42
ASTM D785
Tensile Strength at Break 13.0 MPa
1890 psi
ASTM D638
Tensile Strength, Yield 16.0 MPa
2320 psi
ASTM D638
Elongation at Break 17 %
17 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 1.60 GPa
232 ksi
ASTM D638
Flexural Strength 21.0 MPa
3050 psi
ASTM D790
Flexural Modulus 1.600 GPa
232.1 ksi
ASTM D790
Izod Impact, Notched 1.98 J/cm
3.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C
192 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 53.9 °C
129 °F
Users viewing this material also viewed the following: