Material Notes:
Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingInformation provided by AmericasStyrenics LLC.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 3.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength at Break 19.3 MPa
2800 psi
ASTM D638
Tensile Strength 18.6 MPa
2700 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Tensile Modulus 1.59 GPa
230 ksi
ASTM D638
Flexural Strength 29.0 MPa
4200 psi
ASTM D790
Flexural Modulus 1.59 GPa
230 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
compression molded; ASTM D256
1.44 J/cm
2.70 ft-lb/in
injection molded; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C
192 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
ASTM D648
Vicat Softening Point 100 °C
212 °F
ASTM D1525