Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Hostacomâ„¢ BG722AC Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer LyondellBasell
Trade Name Hostacom™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hostacomâ„¢ BG722AC Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hostacomâ„¢ BG722AC medium high melt flow, 1,700 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer is designed with an excellent balance of stiffness, impact resistance and processability. Uses: Automotive interior partsInformation provided by Basell.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.0 MPa
2470 psi
ASTM D 638
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D 638
Elongation at Break 200 %
200 %
ASTM D 638
Elongation at Yield 6.0 %
6.0 %
ASTM D 638
Flexural Modulus 1.70 GPa
247 ksi
1% Secant, 0.2 in/min; ASTM D790
Izod Impact, Notched 0.849 J/cm
1.59 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C
192 °F
Unannealed; ASTM D648
Shrinkage 1.2 %
1.2 %
Tool, 100x150x3.2 mm; Basell Test Method