Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Americas Styrenics STYRON A-TECH® 1115 High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Americas Styrenics LLC
Trade Name STYRON A-TECH®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Americas Styrenics STYRON A-TECH® 1115 High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product CharacteristicsHigh Gloss/High ImpactConsistent colorabilityEasy processingFood Contact CompliantTypical ApplicationsCustom high Gloss Extruded SheetRefrigeration accessoriesSmall AppliancesInformation provided by AmericasStyrenics LLC.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 2.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102.5
102.5
ASTM D785
Tensile Strength at Break 19.3 MPa
2800 psi
ASTM D638
Tensile Strength 26.9 MPa
3900 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Tensile Modulus 1.83 GPa
265 ksi
ASTM D638
Flexural Strength 35.9 MPa
5200 psi
ASTM D790
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
compression molded; ASTM D256
2.08 J/cm
3.90 ft-lb/in
injection molded; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C
192 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.3 °C
173 °F
ASTM D648
Vicat Softening Point 101 °C
214 °F
ASTM D1525