Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ BMV 102W Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ BMV 102W Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Polyolefin injection molding compound with high flow, good low-temperature impact resistance, and excellent processability for painted, partial painted, and molded-in-color automotive bumper fascia and exterior trim applications.Availability: North America Features: DuctileGood UV ResistanceGood Weather ResistanceHigh FlowLow Temperature Impact ResistancePaintable Uses: Automotive ApplicationsAutomotive Exterior Parts Automotive Exterior TrimAutomotive Specifications: Chrysler MS-DC256 Type BProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ISO 1183/A
Melt Flow 31 g/10 min

@Load 2.16 kg,
Temperature 230 °C
31 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527-2
Flexural Modulus 1.26 GPa
183 ksi
2.52 in, 0.079 in/min; ISO 178
Dart Drop, Total Energy 29.0 J

@Temperature -30.0 °C
21.4 ft-lb

@Temperature -22.0 °F
7.22 ft/sec; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C
192 °F
ISO 75-2/Bf