Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955-89
Melt Flow 15 g/10 min
15 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.7 MPa
3000 psi
ASTM D638-95
Elongation at Break 860 %
860 %
ASTM D638-95
Flexural Strength 24.8 MPa
3600 psi
ASTM D790-95
Flexural Modulus 0.828 GPa
120 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256-93a
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
ASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ASTM D648-95