Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: excellent cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: automotive parts, luggage, totes, bins, carrying cases, appliancesMeets FDA requirements in 21 CFR 177.1520 for all food contact, excluding cooking applications.Description: Pro-fax 8523 super high impact polypropylene copolymer resin is designed for general extrusion or injection molding equipment. This resin is available in pellet form. It has a UL yellow card RTI, which applies to all colors. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched NB
NB
ASTM D256A
Impact Test >= 61.0 J

@Temperature -29.0 °C
>= 45.0 ft-lb

@Temperature -20.2 °F
Montell drop weight impact strength
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
178 °F
ASTM D648
UL RTI, Mechanical with Impact 105 °C
221 °F
Minimum thickness 0.038 inches.
Flammability, UL94 HB
HB
Minimum thickness 0.038 inches.
Copyright © lookpolymers.com All Rights Reserved