Polymer Property : Specific Heat Capacity = 1.55 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.55 J/g-°C
0.370 BTU/lb-°F
Melt
Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled
ISO 7391-PC,MR,(,,)-09-9,GF15Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min15 % Glass fiber reinforcedHigh viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CExtrusionAvailable ..
Specific Heat Capacity 1.55 J/g-°C
0.370 BTU/lb-°F
Melt
Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled
ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva..
Specific Heat Capacity 1.55 - 2.55 J/g-°C
0.370 - 0.609 BTU/lb-°F
Average value: 1.92 J/g-°C Grade Count:6
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Specific Heat Capacity 1.55 - 2.55 J/g-°C
0.370 - 0.609 BTU/lb-°F
Average value: 1.89 J/g-°C Grade Count:17
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..