Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.55 J/g-°C | 0.370 BTU/lb-°F | Melt |
Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min15 % Glass fiber reinforcedHigh viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CExtrusionAvailable .. |
|||
Specific Heat Capacity | 1.55 J/g-°C | 0.370 BTU/lb-°F | Melt |
Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva.. |
|||
Specific Heat Capacity | 1.55 - 2.55 J/g-°C | 0.370 - 0.609 BTU/lb-°F | Average value: 1.92 J/g-°C Grade Count:6 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Specific Heat Capacity | 1.55 - 2.55 J/g-°C | 0.370 - 0.609 BTU/lb-°F | Average value: 1.89 J/g-°C Grade Count:17 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |