Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.55 - 2.55 J/g-°C | 0.370 - 0.609 BTU/lb-°F | Average value: 1.92 J/g-°C Grade Count:6 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Specific Heat Capacity | 1.55 - 2.55 J/g-°C | 0.370 - 0.609 BTU/lb-°F | Average value: 1.89 J/g-°C Grade Count:17 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |