Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.46 - 1.50 J/g-°C | 0.349 - 0.359 BTU/lb-°F | Average value: 1.47 J/g-°C Grade Count:9 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Specific Heat Capacity | 1.30 - 1.50 J/g-°C | 0.311 - 0.359 BTU/lb-°F | DSC |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Specific Heat Capacity | 1.40 - 1.50 J/g-°C | 0.335 - 0.359 BTU/lb-°F | Average value: 1.45 J/g-°C Grade Count:4 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Specific Heat Capacity | 1.00 - 1.50 J/g-°C | 0.239 - 0.359 BTU/lb-°F | Average value: 1.33 J/g-°C Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
Specific Heat Capacity | 1.30 - 1.50 J/g-°C | 0.311 - 0.359 BTU/lb-°F | Average value: 1.44 J/g-°C Grade Count:11 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |