Thermal Properties Metric English Comments
Specific Heat Capacity 1.46 J/g-°C
0.349 BTU/lb-°F
Plaskolite PL-24 Acrylic Resin
For injection molding. An unlubricated version of PL-25 extrusion grade pellets. Highest molecular weight, maximum heat resistance.Information supplied by the manufacturer.
Specific Heat Capacity 1.46 - 1.50 J/g-°C
0.349 - 0.359 BTU/lb-°F
Average value: 1.47 J/g-°C Grade Count:9
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Specific Heat Capacity 1.46 J/g-°C
0.349 BTU/lb-°F
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene
Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH
Specific Heat Capacity 1.46 J/g-°C
0.349 BTU/lb-°F
Diapolyacrylate Acrypet® MF-001 PMMA
Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers.
Specific Heat Capacity 1.46 J/g-°C
0.349 BTU/lb-°F
Diapolyacrylate Acrypet® VH-001 Heat Stabilized PMMA
Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers.
Specific Heat Capacity 1.46 J/g-°C
0.349 BTU/lb-°F
Diapolyacrylate Acrypet® IR H70 Impact Modified PMMA
Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers.
Specific Heat Capacity 1.46 J/g-°C
0.349 BTU/lb-°F
Asahi Kasei Delpet® 560F Acrylic Molding Compound
560F has the highest flow of Delpet® grades, allowing reduced screw load for broad selection of molding conditions. General Delpet® qualities include attractive transparency, elegant luster and c..
Specific Heat Capacity 1.46 J/g-°C
0.349 BTU/lb-°F
Asahi Kasei Delpet® 60N Acrylic Molding Compound
60N is a medium grade of heat resistance and mechanical strength, allowing injection molding through relatively small gates and runners. General Delpet® qualities include attractive transparency, ..
Specific Heat Capacity 1.46 J/g-°C
0.349 BTU/lb-°F
Asahi Kasei Delpet® 80N Acrylic Molding Compound, High Heat Grade
80N has high heat resistance and strength. Recommended for taillight lenses, reflectors, and other auto parts, and general lighting fixtures. General Delpet® qualities include attractive transpar..
Specific Heat Capacity 1.46 J/g-°C
0.349 BTU/lb-°F
Lucite International SW Sanitary Ware Acrylic Sheet
Lucite® SW complies with ISO 7823-1 and EN 263. It is approved by the French ARNOR "NF" quality mark.Information provided by Lucite International