Thermal Properties Metric English Comments
Specific Heat Capacity 1.46 - 1.50 J/g-°C
0.349 - 0.359 BTU/lb-°F
Average value: 1.47 J/g-°C Grade Count:9
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Specific Heat Capacity 1.30 - 1.50 J/g-°C
0.311 - 0.359 BTU/lb-°F
DSC
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Specific Heat Capacity 1.40 - 1.50 J/g-°C
0.335 - 0.359 BTU/lb-°F
Average value: 1.45 J/g-°C Grade Count:4
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Specific Heat Capacity 1.00 - 1.50 J/g-°C
0.239 - 0.359 BTU/lb-°F
Average value: 1.33 J/g-°C Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
Specific Heat Capacity 1.30 - 1.50 J/g-°C
0.311 - 0.359 BTU/lb-°F
Average value: 1.44 J/g-°C Grade Count:11
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..