Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT)abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of p.. |
|||
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T7 Heat Treatment Condition T7 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6 Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Specific Heat Capacity | 0.820 - 0.900 J/g-°C @Temperature 100 - 100 °C |
0.196 - 0.215 BTU/lb-°F @Temperature 212 - 212 °F |
Average value: 0.837 J/g-°C Grade Count:15 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Specific Heat Capacity | 0.850 - 0.900 J/g-°C | 0.203 - 0.215 BTU/lb-°F | |
Hippe PVC-U Polyvinyl Chloride Material at reasonable price, high strength. Used in machine construction as covers, pipes, section, façade elements.Information provided by Hippe. |