Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.860 J/g-°C | 0.206 BTU/lb-°F | Calculated |
Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT)abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of p.. |
|||
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |
|||
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T7 Heat Treatment Condition T7 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Specific Heat Capacity | 0.860 - 0.900 J/g-°C | 0.206 - 0.215 BTU/lb-°F | |
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6 Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Specific Heat Capacity | 0.860 J/g-°C | 0.206 BTU/lb-°F | |
Schott N-KF9 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.860 J/g-°C @Temperature 1093 °C |
0.206 BTU/lb-°F @Temperature 1999 °F |
|
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |