Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.850 J/g-°C | 0.203 BTU/lb-°F | Calculated |
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Specific Heat Capacity | 0.850 J/g-°C @Temperature 100 °C |
0.203 BTU/lb-°F @Temperature 212 °F |
Arlon SQA-TMS-052 |
Arlon Thermabond® R37340X008 Primerless Electronic Adhesive
(discontinued **) Liner: 1 mil FEP; Product: uncured Silicone Rubber; Carrier: 3 mil PTFE coated fiberglas |
|||
Specific Heat Capacity | 0.850 J/g-°C @Temperature 100 - 200 °C |
0.203 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec Frequenta® Steatite Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. Frequenta® has low dielectric loss, but has be.. |
|||
Specific Heat Capacity | 0.850 J/g-°C @Temperature 100 °C |
0.203 BTU/lb-°F @Temperature 212 °F |
Silicone Property; ASTM E 1952 |
Arlon Thermabond® 99A90X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Specific Heat Capacity | 0.850 J/g-°C @Temperature 100 °C |
0.203 BTU/lb-°F @Temperature 212 °F |
Silicone Property; ASTM E 1952 |
Arlon Thermabond® 99A90N008 Primerless Electronic Adhesive
(discontinued **) Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer. |
|||
Specific Heat Capacity | 0.850 - 0.900 J/g-°C | 0.203 - 0.215 BTU/lb-°F | |
Hippe PVC-U Polyvinyl Chloride Material at reasonable price, high strength. Used in machine construction as covers, pipes, section, façade elements.Information provided by Hippe. |