Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.20 J/g-°C | 0.526 BTU/lb-°F | DSC |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Specific Heat Capacity | 2.20 J/g-°C @Temperature 23.0 °C |
0.526 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Specific Heat Capacity | 2.20 J/g-°C | 0.526 BTU/lb-°F | Average value: 2.20 J/g-°C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Specific Heat Capacity | 2.20 J/g-°C | 0.526 BTU/lb-°F | Melt |
Ineos ABS Triax® 1120 ABS + Polyamide Blend (Conditioned) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Specific Heat Capacity | 2.20 J/g-°C | 0.526 BTU/lb-°F | Melt |
Ineos ABS Triax® 1120 ABS + Polyamide Blend (DAM) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Specific Heat Capacity | 2.20 J/g-°C | 0.526 BTU/lb-°F | Melt |
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (Conditioned) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Specific Heat Capacity | 2.20 J/g-°C | 0.526 BTU/lb-°F | Melt |
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (DAM) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Specific Heat Capacity | 2.20 J/g-°C @Temperature 280 °C |
0.526 BTU/lb-°F @Temperature 536 °F |
DSC |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
Specific Heat Capacity | 2.20 J/g-°C | 0.526 BTU/lb-°F | |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
Specific Heat Capacity | 2.20 J/g-°C | 0.526 BTU/lb-°F | DSC |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
Specific Heat Capacity | 2.20 J/g-°C | 0.526 BTU/lb-°F | |
Americas Styrenics Styron® 425 High Impact Polystyrene
(discontinued **) STYRON® 425 impact polystyrene resin is typically used in thin section parts, hot drink cups and cassettes. It offers heat resistance, easy flow, fast cycling, and excellent tensile and flex proper.. |