Thermal Properties Metric English Comments
Melting Point 340 - 360 °C
644 - 680 °F
Average value: 350 °C Grade Count:8
Overview of materials for PEKK, Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M..
Melting Point 262 - 360 °C
504 - 680 °F
Indium Corp. Indalloy® 261 Bismuth-Silver Solder Alloy
Information provided by the manufacturer, Indium Corporation of America.
Melting Point 306 - 360 °C
583 - 680 °F
Average value: 342 °C Grade Count:3
Overview of materials for PEKK, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate..