Material Notes:
Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Density 9.85 g/cc
0.356 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 55.2 MPa
8000 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 37.2 GPa
5400 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 9.00 W/m-K

@Temperature 85.0 °C
62.5 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 262 - 360 °C
504 - 680 °F
Solidus 262 °C
504 °F
Liquidus 360 °C
680 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 89 %
89 %
Germanium, Ge 0.050 %
0.050 %
dopant
Silver, Ag 11 %
11 %
Users viewing this material also viewed the following: